RM

Crystalline type LMF
RM, which is produced by bicomponent spinning of modified polyester through flexible and highly crystallized molecular chain polymerization, can be melted at low temperature (160C), and is not transformed at high temperature after being bonded and formation.

Feature

Good Shape Stability
After bonding and formation, RM is not transformed even at high temperature(100~130C) environments.
Easy Mixing Properties with other Fiber
Homogeneous properties between RM and various fibers make blending easy on line.
Excellent Resilience
The formation of non-woven fabric made with RM is simple and excellent.
Good Strength
RM has good bonding strength and high tearing strength.

Applications

Automotive Use
Headliner, Doortrim, Floor carpet, Trunk, Rearshelf

Production item

Type

Luster

De

Length(mm)

Melting Point

Remarks

LMF50

SD

4

64

164℃

Crystalline